posted on 2024-06-24, 04:01authored byLi Ning, Chao Wang, Nanxiang Jia, Zhiqiang Ma, Yujie Dang, Chao Sun, Hongliang Du, Zhuo Xu, Fei Li
See the supplementary material for the details of structure parameters of PSCCs (Table. S1); the photographs of PSCCs (Fig. S1); the conversion between Ep and Erms of electric field for ACP and DCP. (Fig. S2); the conversion between Ep and Erms of alternating electric fields used in this work (Table S2); the polarized light microscope patterns of domain morphology at P/A 45{degree sign} for sample with 500 μm (Fig. S3); the performance parameters of PSCCs (Table S3); the polarized light microscope patterns of domain morphology at P/A: 0{degree sign} for 500 μm samples by DCP and ACP (Fig. S4); the temperature dependence of d_33^* for ACP and DCP PSCCs with a thickness of 600 μm (Table S4).