posted on 2025-06-05, 12:03authored byTakahiro Yoshino, Siyi Tang, Md Sarker, E M K Ikball Ahamed, Zhiqiang Liao, Hiroyasu Yamahara, Hitoshi Tabata, Munetoshi Seki
The experimental data of XPS spectra of the Al:YIG bulk target, M-H hysteresis loops, temperature dependence of the imaginary part of the AC magnetic susceptibility, an MCD spectrum at the wavelength region of 375-500 nm, and magnetic field dependence of MCD of the Al:YIG film are shown.